1,Technischer Index

2,Description of molecular sieve: it has strip shape and spherical shape, small diameter and small pore diameter. It is divided into 3A, 4A and 5A, and has uniform size. It has strong adsorption capacity, drying capacity, separation capacity and strong thermal shock stability. It has the advantages that other adsorbents do not have. It can be used as desiccant, selective adsorbent, catalyst, ion exchanger, etc. Molecular sieves can be recycled. They are usually regenerated and reused by reheating and purging or evacuation. Molecular sieves are aluminum silicate compounds, not chemicals, non-toxic and environmental friendly.
3, Eigenschaften des Molekularsiebs:
1) Hohe Adsorptionskapazität
2) Hohe Festigkeit
3) Hohe Verschleißfestigkeit und niemals Pulverisierung
4) Hohe Trennleistung
5) Die Nutzungsdauer beträgt mehr als 3 Jahre
4, Zweck
1) Trocknen verschiedener Flüssigkeiten
2) Adsorption und Trennung verschiedener Gase
3) Trockenmittel, Katalysator und Adsorptionsmittel verschiedener Trocknungsgeräte, Trenngeräte und Reinigungsgeräte
5, Bewerbungsbild


6, gutes Feedback des Produktnutzungseffekts, die Produkte wurden nach Südkorea, Japan, Pakistan exportiert
7, Wir sind ein professioneller Anbieter, der Kunden mit kostenloser Produkttechnologie, Verwendung und anderen Problemen versorgen kann
Möchten Sie einen professionellen Anbieter von Molekularsiebprodukten finden?
Möchten Sie einen stabilen und glaubwürdigen Lieferanten finden?
Then please contact with us
Kontaktiere mich:
E-Mail:wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / FAX: 86-0533-4188518
Rose: plus 86-13275332819(WeChat/WhatsApp-Nummer)
Beliebte label: Molekularsieb, China, Hersteller, Lieferanten, Fabrik, Verwendung, Eigentum