Säure-resistierende Ziegelstein für Schornsteinis made of pottery clay and clay as the main raw materials, through mixing, molding, firing and other processes to produce acid resistant products. The product has high acid resistance and is not easy to be oxidized under normal temperature. Besides hydrofluoric acid and thermal phosphoric acid, it has excellent anti-corrosion effect on many acid substances. It is Häufig in elektrischer Leistung, Metallurgie und anderen Schornsteinen und Abzügen . verwendet
1. Funktionen vonSäure-resistierendes Ziegelstein für Schornstein:
1) hohe Säureresistenz, größer oder gleich 97%, gute Antikorrosionseffekt auf die meisten Säure-Produkte
2) Veränderung kleiner Volumen, gute Korrosionsbeständigkeit
3) Farbe ist lila rot
Oder
The main component of acid resistant brick is SiO2, which forms a lot of polyaluminal Andalusite in the process of high temperature sintering. It is a kind of material with high acid resistance. The acid resistant brick has compact structure (density>=2.4g/cm3), low water absorption, and can withstand any concentration of acid medium Bei Raumtemperatur . sind die Produkte in schwere Ziegel- und leichte Ziegelsteine unterteilt, die beide eine gute Säure -Resistenz -Atmosphäre, Lufterosion und Erosionsleistung aufweisen.
Oder
4. Unser Unternehmen ist frei, den Benutzern Technologie, Nutzung und andere Dienste zu bieten. .
Möchten Sie einen professionellen Anbieter von feuerfesten Produkten finden?
Möchten Sie einen stabilen und glaubwürdigen Lieferanten finden?
Dann wenden Sie sich bitte an uns
Kontaktieren Sie mich:
E -Mail: wp@cnjingganrefractory.com/sdwenping@163.com
Tel.: 86-0533-4188518 / fax: 86-0533-4188518
Rose: +86-13275332819 (WeChat/WhatsApp -Nummer)